Chromium-doped Yttrium-Aluminum Garnet (Cr4+:YAG)


Introduction | Main Properties | Standard Specicications | Notes



III. Standard Specifications


Cr4+ doping level 0.5 ~ 3.5 mol%
Standard Aperture f 2~25 mm or 2x2 ~ 18x18 mm2
Initial Transmission 1.0% ~ 99.0%
Wavefront Distortion l/8 @633 nm
Flatness l/10 @633 nm
Parallelism < 10 arc seconds
Perpendicularity < 5 arc minutes
Scratch/Dig Code 10/5 per MIL-O-13830A
Barrel Finish 50 - 80 micro-inch (RMS)
Anti-Reflection Coating R < 0.1% @1.064 mm per surface